All the major electronic/microelectronic adhesive suppliers have
screenable Ag epoxies you could sort of use for this, but I would be a
bit sniffy about it.
Its been done before, but personally I would not recommend it except
as a short term/prototyping type fix. Not really good for a long term
high reliability assembly, probing on to Ag epoxy is not necessarily
going to produce a consistent result either. Does your customer have
prior experience on this assembly showing results are good enough for
the intended application?
Mike
----- Original Message -----
From: "Hans Rohr" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, July 26, 2000 2:10 AM
Subject: [TN] Plugging Vias With Conductive Epoxy
> One of our customers wants us to plug vias (.016-.020") with a
> conductive epoxy material. The board is finished with white tin so
> plugging with solder is out. The vias do not have to be completely
> filled but the plugs must be strong enough to withstand test probe
> pressure. The epoxy filled vias will be used as test points. We
have
> used carbon and silver epoxy on conductive surfaces but never to
plug
> holes. Has anyone ever done this and can you suggest a conductive
epoxy
> that can be screened on?
>
> Hans Rohr
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV
1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|