Gabi,
        I'm afraid I am not much of an expert in adhesive cleaning.  (I
don't use it very much).  But I do know that IPA will leave a film of glue
all over the board.  I have found that the particular Loctite glue we use
will come off in a saponified ultrasonic cleaner.  (Remember to use sweeping
ultrasonic if there are components on the board already!)

Thanks

Ryan Grant
Advanced Technology Engineer
MCMS
(208) 898-1145
[log in to unmask]


> -----Original Message-----
> From: Bogdan Gabi [SMTP:[log in to unmask]]
> Sent: Tuesday, September 19, 2000 9:08 AM
> To:   [log in to unmask]
> Subject:      Re: [TN] Missprints
>
> Thank you,Ryan!
> what about adheasive cleaning and OSP?
> Gaby
>
> > ----------
> > From:         Ryan Grant[SMTP:[log in to unmask]]
> > Reply To:     TechNet E-Mail Forum.;Ryan Grant
> > Sent:         ???? ????? 19 ?????? 2000? 17:20
> > To:   [log in to unmask]
> > Subject:      Re: [TN] Missprints
> >
> > Gabi,
> >         I'm afraid that if you want to remove the flux in the solder
> > paste,
> > you must use a solvent that also removes the OSP coating.  So joint the
> > rest
> > of us in the frothing sea and use IPA.  Just make sure you reprint that
> > board as soon as it is clean.  (Works great!).  By the way, if you use
> > no-clean, you will need to use an ultrasonic cleaner to avoid
> solderballs.
> > It is impossible to completely clean solder paste out of vias without
> it.
> >
> > Thanks
> >
> > Ryan Grant
> > Advanced Technology Engineer
> > MCMS
> > (208) 898-1145
> > [log in to unmask]
> >
> >
> > > -----Original Message-----
> > > From: Bogdan Gabi [SMTP:[log in to unmask]]
> > > Sent: Tuesday, September 19, 2000 5:00 AM
> > > To:   [log in to unmask]
> > > Subject:      [TN] Missprints
> > >
> > > Dear TechNetters,
> > > Which solvents and methods are the best for missprint cleaning on OSP
> > > coated
> > > boards?
> > > Thank you,
> > > Gaby
> > >
> > > ##############################################################
> > > TechNet Mail List provided as a free service by IPC using LISTSERV
> 1.8d
> > > ##############################################################
> > > To subscribe/unsubscribe, send a message to [log in to unmask] with
> > > following text in
> > > the body:
> > > To subscribe:   SUBSCRIBE TECHNET <your full name>
> > > To unsubscribe:   SIGNOFF TECHNET
> > > ##############################################################
> > > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> > > additional
> > > information.
> > > If you need assistance - contact Keach Sasamori at [log in to unmask] or
> > > 847-509-9700 ext.5315
> > > ##############################################################
> >
> > ##############################################################
> > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
> > ##############################################################
> > To subscribe/unsubscribe, send a message to [log in to unmask] with
> > following text in
> > the body:
> > To subscribe:   SUBSCRIBE TECHNET <your full name>
> > To unsubscribe:   SIGNOFF TECHNET
> > ##############################################################
> > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> > additional
> > information.
> > If you need assistance - contact Keach Sasamori at [log in to unmask] or
> > 847-509-9700 ext.5315
> > ##############################################################
> >
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2