TECHNET Archives

July 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 12 Jul 2007 14:09:31 EDT
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Parts/Attachments:
text/plain (38 lines)
 
 
In a message dated 7/11/2007 4:18:48 PM Eastern Daylight Time,  
[log in to unmask] writes:

I'm  looking for comments from those who have any experience in attempting 
to  apply conformal coatings to a hot assembly. By hot I would say equal to 
or  less than the recommended cure temperature for the particular coating. 
I'd  be interested in any positives or negatives to having a hot assembly 
while  applying the coating. Thanks.

=========
 
It depends on the type of coating and the type of coating  process.  A 
solvent based coating will tend to flash off faster and  "freeze" in place in a 
spray or selective type application.  This can be  good for very tight keep-out 
clearances and can be bad if you expect coating to  flow under devices, etc.  
Most silicone coatings will have the opposite  reaction.  The heat will reduce 
the viscosity and the coating will flow  further and wet better.
 
Jon Moore




************************************** Get a sneak peak of the all-new AOL at 
http://discover.aol.com/memed/aolcom30tour

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2