TECHNET Archives

June 2016

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 17 Jun 2016 12:17:23 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
Victor Hernandez <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (42 lines)
Greg,

   Thank you very much for sharing.   I was interested in the ball/sphere size.   Do you know if there is a ball/sphere chart for the different solder types.   I will also reach out to Kris Roberson at IPC.

Victor,

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Greg Munie
Sent: Thursday, June 16, 2016 2:49 PM
To: [log in to unmask]
Subject: Re: [TN] Solder fines

Do you mean defined solder particles as opposed to the loose solder debris that might accompany them?

Type 6 is the smallest generally commercial powder. But there has been talk about smaller. (From my experience at Kester MANY years ago 6 was hard enough.)

And little non-spherical pieces do tend to infest any powder of any standard size.

I think Kris Roberson is currently IPC liaison for the committee that specifies size and particle distribution.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Thursday, June 16, 2016 1:19 PM
To: Technet
Subject: [TN] Solder fines

Fellow TechNetters:

What is the smallest solder fines that is currently being used in today LF processes?.

Victor,


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2