TECHNET Archives

March 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
"Bloomquist, Ken" <[log in to unmask]>
Date:
Wed, 20 Mar 2002 09:56:53 -0800
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Bloomquist, Ken" <[log in to unmask]>
Parts/Attachments:
text/plain (135 lines)
I think Phil is on the right track. Get a couple of these coats and start
washing and testing. The only thing you don't have control over is the type
of washing your employees will do at home, i.e. temperature, amount of
detergent, type of detergent, drying temperature, fabric softeners, etc.  I
guess you could have each person take your test coats home and wash them,
test them and pass them on to the next. There are a lot of variables though.

Ken Bloomquist
Sr. Principal Process Engineer

GENERAL DYNAMICS
9845 Willows Rd. NE.
Redmond, WA 98052-2540
425-556-4554
[log in to unmask]
www.gd-ots.com


 -----Original Message-----
From:   Phil Nutting [mailto:[log in to unmask]]
Sent:   Wednesday, March 20, 2002 6:48 AM
To:     [log in to unmask]
Subject:        Re: [TN] ESD Smocks

I saved the threads from May and June of 2000 regarding ESD smocks for my
own reference.  Just reviewed them and there are arguments pro and con for
wearing and washing.

From the Electrostatic Discharge Association's web page http://www.esda.org/

This standard is listed for ESD garments.

ANSI ESD STM2.1-1997: Resistance Test Method for Electrostatic Discharge
Protective Garments
This Standard Test Method provides test methods for measuring the electrical
resistance of garments used to control electrostatic discharge. It covers
procedures for measuring sleeve-to-sleeve and point-to-point resistance.

Hope this is of some use.  I have not selected a side of the fence to sit
on.

Phil Nutting


-----Original Message-----
From: Lee Whiteman [mailto:[log in to unmask]]
Sent: Wednesday, March 20, 2002 9:04 AM
To: [log in to unmask]
Subject: Re: [TN] ESD Smocks


Kathy,

I would be very skeptical about using these types of ESD smocks. The ones
that I'm familiar with would never survive washing at home.

I've seen companies have their employees wear ESD smocks and shoes outside
of their facility, wash their ESD apparel at home, and wonder why they have
an ESD problem. I'm with Ron Dieselberg. Keep your ESD material controlled
within your facility. That's really the only way you can control the quality
of the ESD smocks.

Hope this helps. Good Luck.

Lee Whiteman
Senior Manufacturing Engineer
E-Mail: [log in to unmask] <mailto:[log in to unmask]>
Ph: (610) 362-1200 x208
Fax: (610) 362-1290



> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Kathy Kuhlow
> Sent: Tuesday, March 19, 2002 2:50 PM
> To: [log in to unmask]
> Subject: [TN] ESD Smocks
>
>
> My company has considered changing to an ESD smock that the
> operator can take home.  Supposedly the smock can be washed
> regularly w/o bleach and also dried with fabric softeners.  The
> smock is good for 50-100 washes.  Something sounds wrong here.
> Is anyone else out there using smocks like this, likes/dislikes, etc.?
>
> TIA
>
> Kathy
>

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2