hi,
are you sure that it is 3m rtv 738? i'm only familiar with dow corning's rtv 738. try giving them a call.
phil
-----Original Message-----
From: <Peter George Duncan> [mailto:[log in to unmask]]
Sent: Tuesday, March 20, 2001 6:12 PM
To: [log in to unmask]
Subject: [TN] Solvent for RTV738
Hi, TechNetters,
I am trying to find a solvent for removing 3M's RTV 738 that has been used
for bonding components to a number of boards, or to each other. Any
suggestions?
I have tried 3M themselves and they have no solvent of their own apart from
"Citrus Base Adhesive Remover" that 'may soften' it enough to peel it off,
but this seems pretty indefinite.
Thanks in hope
Pete Duncan
Asst Principal Engineer
Singapore Technologies Aerospace
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|