hi, are you sure that it is 3m rtv 738? i'm only familiar with dow corning's rtv 738. try giving them a call. phil -----Original Message----- From: <Peter George Duncan> [mailto:[log in to unmask]] Sent: Tuesday, March 20, 2001 6:12 PM To: [log in to unmask] Subject: [TN] Solvent for RTV738 Hi, TechNetters, I am trying to find a solvent for removing 3M's RTV 738 that has been used for bonding components to a number of boards, or to each other. Any suggestions? I have tried 3M themselves and they have no solvent of their own apart from "Citrus Base Adhesive Remover" that 'may soften' it enough to peel it off, but this seems pretty indefinite. Thanks in hope Pete Duncan Asst Principal Engineer Singapore Technologies Aerospace --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 --------------------------------------------------------------------------------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------