Hi Ruby,
Yes, there are some concerns about PTVs partially filled with solder. The
transition from solder-filled to non-solder-filled produces a stress riser in
the Cu PTV barrel walls. This is of no practical concern for applications for
which the thermal cyclic environment is not severe; for severe environments,
e.g., automotive, military, some satellites, this stress riser can be
enoughto cause premature failure.
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask], Website: www.engelmaier.com
In a message dated 6/28/00 11:19:14, [log in to unmask] writes:
>Hello all:
>We try to fully or partially fill the via holes (<0.025" diameter) with
>solder due to the process. I'm wondering that if there are some concerns
>(such as fatigue).
>Any information are very welcome. Thanks a lot!
>R.H.
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|