TECHNET Archives

June 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
"Howieson, Rick" <[log in to unmask]>
Date:
Thu, 29 Jun 2000 08:47:36 -0600
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Howieson, Rick" <[log in to unmask]>
Parts/Attachments:
text/plain (67 lines)
Werner,
What about tented vias using LPISM. And...is this done by flooding using
a dot pattern for the vias only? We typically tent using DFSM however,
at times there are requirements for LPI.
TIA,
Rick Howieson
http://www.gt-corp.com

>-----Original Message-----
>From:  Werner Engelmaier [SMTP:[log in to unmask]]
>Sent:  Thursday, June 29, 2000 7:17 AM
>To:    [log in to unmask]
>Subject:       Re: [TN] Filled via holes
>
>Hi Ruby,
>Yes, there are some concerns about PTVs partially filled with solder. The
>transition from solder-filled to non-solder-filled produces a stress riser in
>the Cu PTV barrel walls. This is of no practical concern for applications for
>which the thermal cyclic environment is not severe; for severe environments,
>e.g., automotive, military, some satellites, this stress riser can be
>enoughto cause premature failure.
>
>Werner Engelmaier
>Engelmaier Associates, L.C.
>Electronic Packaging, Interconnection and Reliability Consulting
>7 Jasmine Run
>Ormond Beach, FL  32174  USA
>Phone: 904-437-8747, Fax: 904-437-8737
>E-mail: [log in to unmask], Website: www.engelmaier.com
>
>In a message dated 6/28/00 11:19:14, [log in to unmask] writes:
>>Hello all:
>>We try to fully or partially fill the via holes (<0.025" diameter) with
>>solder due to the process. I'm wondering that if there are some concerns
>>(such as fatigue).
>>Any information are very welcome. Thanks a lot!
>>R.H.
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in
>the body:
>To subscribe:   SUBSCRIBE TECHNET <your full name>
>To unsubscribe:   SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>If you need assistance - contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2