Subject: | |
From: | |
Reply To: | TechNet E-Mail Forum. |
Date: | Wed, 8 Dec 1999 18:41:51 -0500 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
Does anyone have a $ value regarding Ni/Pd/Au v.s. electrolytic Ni/Au?
Many thanks.
joyce
At 07:07 AM 12/8/99 -0700, you wrote:
>Paul,
> I suspect the use of Palladium is to prevent "black pad" since it has
>been found to occur during the immersion gold process. With a Palladium
>layer on the nickel, hyper corrosion of the nickel should not occur (in
>theory). (it still sounds expensive).
>
>
> Thanks
>
>Ryan Grant
>Process Development Engineer
>MCMS
>(208) 898-1145
>FAX (208) 898-2789
>[log in to unmask]
>
>
>
>
>
>
>No problems 1-5 Darrel, just ask him why standard (flash) NiAu would not
>be
>sufficient .
>>From distance i can't see the need for Pd instep expense.
>Check net's archives , all there
>
>pk
>
>-----Original Message-----
>From: Darrel Therriault [mailto:[log in to unmask]]
>Sent: Tuesday, 7 December 1999 4:59
>To: [log in to unmask]
>Subject: [TN] Ni/Pd/Au
>
>
>TechNet,
>
>A PWB supplier is recommending a Ni/Pd/Au finish for .062" and .093"
>FR-4
>PWB
>with mixed PTH/SMT components, as well as press fit connectors.
>
>Any comments/guidance, pro or con, regarding :
>
>1. Intermetalics
>2. Rework cycles
>3. Gold embriddlement
>4. Fine pitch or BGA components
>5. Pressfit
>
>All info appreciated.
>
>Regards.......DT
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
>following
>text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
>additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask]
>or
>847-509-9700 ext.5365
>##############################################################
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
>following text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
>additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask]
>or
>847-509-9700 ext.5365
>##############################################################
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>847-509-9700 ext.5365
>##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|