TECHNET Archives

May 2015

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Frank Seter <[log in to unmask]>
Date:
Tue, 5 May 2015 11:23:53 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Subject:
From:
Steve Gregory <[log in to unmask]>
Message-ID:
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (58 lines)
Hi Frank,

It's been quite some time ago (1990), but we had a fire on the production
floor at a company I worked for out in California. We had worked a
Saturday, and when it was quitting time our wave operator at the time, who
was also responsible for our cleaners, didn't shut everything off for our
inline aqueous cleaner. Well it was a polypropylene cleaner and we believe
something failed because it wound-up boiling all of the water out of the
wash tank and eventually caught on fire very early (about 2:30am) Sunday
morning:

 http://stevezeva.homestead.com/Comptronix_Fire.jpg

I got called in at around 6:30am. At first I thought somebody at work was
just playing a joke. but when I finally got there and saw all the fire
trucks I knew it was for real. We all pitched in and started cleaning up.
We still had our Detrex inline freon cleaner, so we ran all the boards that
were still in WIP on the floor through that cleaner. Anything that we had
an electrical test on was re-tested again. We notified our customers of
what had happened and what we were doing with the product that was on the
floor. After all was said and done the only board we lost were ones that
were sitting in a tilt rack on a table close to the cleaner.

We called a disaster clean-up company to come in Monday morning and believe
it or not we were back in production on Wednesday. A lot of work to be sure!

Steve

On Fri, May 1, 2015 at 1:37 PM, Frank Seter <[log in to unmask]> wrote:

> Does anyone have data or experience with Chlorides and Sulfates generated
> during a fire damaging circuit boards?
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>

-- 


This email and any attachments are only for use by the intended 
recipient(s) and may contain legally privileged, confidential, proprietary 
or otherwise private information. Any unauthorized use, reproduction, 
dissemination, distribution or other disclosure of the contents of this 
e-mail or its attachments is strictly prohibited. If you have received this 
email in error, please notify the sender immediately and delete the 
original. 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2