TECHNET Archives

June 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Stadem, Richard D.
Date:
Thu, 5 Jun 2008 11:30:08 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (55 lines)
Was it a stainless steel brush being used to improve the Huntron's
electrical probe contact? 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Leland Woodall
Sent: Thursday, June 05, 2008 9:15 AM
To: [log in to unmask]
Subject: [TN] Stainless Steel Contamination Question - Source Nailed!

Everyone,

After checking every filter, every transfer belt, every reflow oven, and
most every square inch of the building, I was able to identify the
source of the 10 micron stainless steel that has been giving us such a
headache.  Just in case anyone ever has the same problem, I thought I'd
share the solution with our group.

To refresh your memory, we were finding this stuff on top of components,
and later inside our Huntron X-Y table inspection machines.  We did
everything but take a hatchet to the Huntrons, and there was nothing
found (of course).

While one of the Huntron machine's operator was gone to lunch, I decided
to check an item she had left behind on her workstation.  I took it to
the lab, placed it beneath the microscope, and was astonished to find an
identical match to our contamination woes.

Before I let the cat out of the bag, does anyone want to venture a
guess?

Leland

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2