On local fid's try and keep parts away that may reflect light back into the
camera. Parts that are white or have a shiny surface make it difficult for
the camera to capture fid's. I have also seen issues when the fid is a
similar size as the copper balancing on the assembly rail. I do not know if
that was a board house issue or a designer used a similar size fid as the
board house to balance the copper, could have been just dumb luck. I have
added notes to manufacturing instructions not to use copper dots on the
assembly rail to avoid any confusion.
Ted T.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ahne Oosterhof
Sent: Thursday, June 05, 2008 9:46 AM
To: [log in to unmask]
Subject: Re: [TN] Fiducial solder resist clearance
Don't ask what the designers prefer, ask what the customers (users) prefer.
The most common size/shape is a 1mm (0.040") circle. It is prefered to have
a flat finish, so that the vision cameras do not get confused by variations
in reflections and glare. That is also why solder mask is not put up to the
edge of the fiducial. Any error in putting down the solder mask will cover
part of the fiducial.
Have fun,
Ahne.
Fine Line Stencil, Inc.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas McCall
Sent: Wednesday, 04 June, 2008 03:14
To: [log in to unmask]
Subject: [TN] Fiducial solder resist clearance
Hi,
When desiging the PWB for fiducials, what is the experience of having the
solder resist up to the edge of the fiducial pad.
If the recommended clearance window round (2-3 x fiducial radius) the
fiducial is not maintained does this in general cause excessive vision
system problems, - looking at the solder resist compared to looking at the
laminate material.
I understand that this clearance should be left with no resist and leaving
the bare PWB laminate and etched fidicial feature.
What is the prefered fiducial shape used by most designers?
Thanks in advance for any information.
D. McCall.
_________________________________________________________________
Great deals on almost anything at eBay.co.uk. Search, bid, find and win on
eBay today!
http://clk.atdmt.com/UKM/go/msnnkmgl0010000004ukm/direct/01/
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|