TECHNET Archives

January 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vp2c0-0000UDC; Mon, 27 Jan 97 19:45 CST
Old-Return-Path:
Date:
Mon, 27 Jan 1997 17:35:46 -0800
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/9687
TO:
Return-Path:
<TechNet-request>
From [log in to unmask] Tue Jan 28 13:
16:09 1997
Resent-Message-ID:
<"d4GcI2.0.I17.peLxo"@ipc>
Subject:
From:
Bob Metcalf <[log in to unmask]>
X-Loop:
Cc:
X-Mailer:
Novell GroupWise 4.1
Message-Id:
Parts/Attachments:
text/plain (45 lines)
Jon, if you would like to contact me, I would be happy to discuss further
with you. We have done a lot of work in this area.

Bob Metcalf
Morton Electronic Materials
714-730-8356

>>> "Hemstad, Jon (MN51)" <[log in to unmask]>
01/27/97 12:04pm >>>
I am looking for information on matte-finish solder masks.  My company is 
going to a no clean process and the matte-finish will help control solder 
balls.  What measure is used to gauge the matte-finish and how does a 
company control and measure the quality of the matte-finish coming in? 
Any 
information would be appreciated.

Jon Hemstad

[log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.       
*
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact  
*
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2