Jon, if you would like to contact me, I would be happy to discuss further with you. We have done a lot of work in this area. Bob Metcalf Morton Electronic Materials 714-730-8356 >>> "Hemstad, Jon (MN51)" <[log in to unmask]> 01/27/97 12:04pm >>> I am looking for information on matte-finish solder masks. My company is going to a no clean process and the matte-finish will help control solder balls. What measure is used to gauge the matte-finish and how does a company control and measure the quality of the matte-finish coming in? Any information would be appreciated. Jon Hemstad [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************