TECHNET Archives

April 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset="us-ascii"
Old-Return-Path:
Date:
Thu, 17 Apr 1997 09:30:45 -0400
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/12057
X-Sender:
TO:
Return-Path:
<TechNet-request>
X-Loop:
Resent-Message-ID:
<"amQXy2.0.eC7.fYULp"@ipc>
Subject:
From:
"D.C.Whalley" <[log in to unmask]>
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wHnBa-000BilC; Thu, 17 Apr 97 04:08 CDT
From [log in to unmask] Thu Apr 17 08:
39:11 1997
X-Mailer:
Windows Eudora Light Version 1.5.4 (16)
Message-Id:
Parts/Attachments:
text/plain (40 lines)
Does anyone have experience with using wave solder profiling instruments,
e.g. the
Mole WaveRIDER and Alpha solder wave optimiser?

Are there any other instruments out there?

Do these instruments measure the critical parameters in wave solder process
setup?

Have you found them usefull/reliable/easy to use?

Are there any other factors I should be looking for in purchasing one?

Thanks in advance for your help.

David Whalley
Manufacturing Engineering Department
Loughborough University
Loughborough
Leics LE11 3TU
UK

Tel. +44(0)1509 222930
Fax. +44(0)1509 267725

[log in to unmask]
http://info.lboro.ac.uk/departments/en/STAFF/David_Whalley/index.html

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2