YOU WROTE:
>Does anyone have experience with using wave solder profiling
instruments,>e.g. the Mole WaveRIDER and Alpha solder wave optimiser?
>
>Are there any other instruments out there?
>
>Do these instruments measure the critical parameters in wave solder process
setup?
>
>Have you found them usefull/reliable/easy to use?
>
>Are there any other factors I should be looking for in purchasing one?
>
>Thanks in advance for your help.
>
>David Whalley
>Manufacturing Engineering Department
>Loughborough University
>Loughborough
>Leics LE11 3TU
>UK
>
>Tel. +44(0)1509 222930
>Fax. +44(0)1509 267725
>
>[log in to unmask]
>http://info.lboro.ac.uk/departments/en/STAFF/David_Whalley/index.html
We use an ECD M.O.L.E. for all our solder profiling but are considering one
of these also. Hope you get some good replies to your question to help in
our evaluation also.
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************