TECHNET Archives

September 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
arnaud grivon <[log in to unmask]>
Date:
Mon, 25 Sep 2006 11:57:09 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Kane, Amol (349)" <[log in to unmask]>
Subject:
From:
"Kane, Amol (349)" <[log in to unmask]>
X-cc:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (118 lines)
Hi Arnaud,
Thank you for your interest. I shall put up the relevant information on the forum shortly as I will be at  SMTA this week

Amol Kane
M.S (Industrial Eng.)
Process Engineer
Harvard Custom Manufacturing, Inc. 
941 Route 38  Owego, NY 13827
Phone: (607) 687-7669 x349
Fax: (607) 687-9733
[log in to unmask]
www.harvardgrp.com

 -----Original Message-----
From:   arnaud grivon [mailto:[log in to unmask]] 
Sent:   Monday, September 25, 2006 10:59 AM
To:     Kane, Amol (349)
Subject:        [Fwd: Re: [LF] Copper Pad Peel Strength]
Importance:     High

Hello Amol,

I keep interest in the thread you initiated on the TechNet forum dealing 
with PCB pad peel-off in repair.
What I would like to know is what PCB base material is concerned and 
what kind of BGA, as well as why the components needed to be repaired.
Could you share these information with me?

I thank you in advance.

Best regards,

Arnaud Grivon

-------- Message original --------
Sujet:  Re: [LF] Copper Pad Peel Strength
Date:   Wed, 30 Aug 2006 12:02:43 +0200
De:     arnaud grivon <[log in to unmask]>
Pour:   Kane, Amol (349) <[log in to unmask]>
Références: 
<[log in to unmask]>



Amol,

Not sure if you got my request for additional information about your 
problem, namely BGA and PCB type and PCB base material reference. Could 
you provide these information?
Other questions by TechNet members are also of interest for the better 
understanding of the phenomenon.

Best regards,

A. Grivon


Kane, Amol (349) a écrit :
> Dear Technetters,
> We are having instances where copper pads (Under BGAs) are being lifted off ENIG Boards almost too easily during rework. We use the same thermal profile on each board (for the same component removal) and only some show this phenomenon. Is there a test or standard to test the copper adhesion @ incoming to see whether it's the fab (i.e. are the boards coming to us with poor copper adhesion strength to being with) or the process that's doing this. The board is heated upto 120 C when the component is reflowed for removal. Also, is there data to show the decrease in Cu adhesion strength with temp?
>
> Thanks,
>
> Amol Kane
> M.S (Industrial Eng.)
> Process Engineer
> Harvard Custom Manufacturing, Inc. 
> 941 Route 38  Owego, NY 13827
> Phone: (607) 687-7669 x349
> [log in to unmask]
> www.harvardgrp.com
>
>
>
>
> CONFIDENTIALITY NOTICE: 
> This e-mail, and any attachments, is for the sole use of the intended 
> recipient(s) and may contain information that is confidential and 
> protected from disclosure under the law. Any unauthorized review, use, 
> disclosure, or distribution is prohibited. If you are not the intended 
> recipient, please contact the sender by reply e-mail, and delete/destroy 
> all copies of the original message and attachments. 
> Thank you.
>
> -------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Leadfree
> To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
> Search previous postings at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -------------------------------------------------------------------------------
>   







CONFIDENTIALITY NOTICE: 
This e-mail, and any attachments, is for the sole use of the intended 
recipient(s) and may contain information that is confidential and 
protected from disclosure under the law. Any unauthorized review, use, 
disclosure, or distribution is prohibited. If you are not the intended 
recipient, please contact the sender by reply e-mail, and delete/destroy 
all copies of the original message and attachments. 
Thank you.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2