TECHNET Archives

January 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet (E-mail)" <[log in to unmask]>
Date:
Tue, 13 Jan 2004 15:56:39 -0800
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "MacConnell, Richard B (ES)" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"MacConnell, Richard B (ES)" <[log in to unmask]>
Parts/Attachments:
text/plain (28 lines)
TechNet team,

I have an application where a LCCC (CTE = 7.6 ppm/°C) is to be soldered on
to a Rogers Corp Duroid substrate (CTE = 24 ppm/°C).  I know how to do the
length differential calculation over temperature, but what criteria do I use
to say whether the differential is OK or not OK?  I could also do a stress
calculation on the solder joints, but I don't have a value for Young's
Modulus of the solder to plug in.

If you have rules of thumb or past experience to share, I'd appreciate
hearing from you.

Thanks,

Rich MacConnell
Mechanical Engineer
Northrop-Grumman

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2