For low volume production, we buy MIL approved acrylic in aerosol cans.  No
spray gun required.

Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879


        -----Original Message-----
        From:   Dehoyos, Ramon [SMTP:[log in to unmask]]
        Sent:   Tuesday, May 14, 2002 2:48 PM
        To:     [log in to unmask]
        Subject:        [TN] Conformal Coating

                 My question is about conformal coating. We want to manualy
        conformal coat boards using a spray gun.  Does anybody  have
knowledge of a
        gun that sprays pure coating without any atomization of the coating
and that
        internally have very few        parts, in case it clogs, and needs
to be
        cleaned.
                Regards,
                Ramon


----------------------------------------------------------------------------
-----
        Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL
        To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
        Search the archives of previous posts at:
http://listserv.ipc.org/archives
        Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
        information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315

----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2