Hello Rich,
The component vendor does not seem to understand the soldering process.
You need to reflow to suit the solder paste not the metal being soldered
to.
regards,
Phil.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Richard Kraszewski
Sent: Thursday, 26 October 2006 2:47 PM
To: [log in to unmask]
Subject: [TN] Backward Compatibility of Tin Electroplating
Does anyone have any reason to suspect that tin electroplated SM
components being soldered with a 63/37 solder paste require a profile
that must exceed the reflow temperature of tin?
Being told by a component vendor this is the case. I would totally
discount this but seem to recall reading this more than once on some
other component Tech data sheets. I can't explain why this would be
necessary, but.....
Any thoughts would be appreciated.
Rich K / Kimball
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
Disclaimer :
The contents of this e-mail including any attachments are intended only
for the person or entity to which this e-mail is addressed. If you are not,
or believe you may not be, the intended recipient, please advise the sender
immediately by return e-mail, delete this e-mail and destroy any copies.
Tenix does not warrant nor guarantee that this email communication is free
from errors, virus, interception or interference.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|