TECHNET Archives

October 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Richard Kraszewski <[log in to unmask]>
Date:
Thu, 26 Oct 2006 16:47:11 +1000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, DUTTON Phil <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="US-ASCII"
From:
DUTTON Phil <[log in to unmask]>
Parts/Attachments:
text/plain (66 lines)
Hello Rich,

The component vendor does not seem to understand the soldering process.
You need to reflow to suit the solder paste not the metal being soldered
to.

regards,
Phil.


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Richard Kraszewski
Sent: Thursday, 26 October 2006 2:47 PM
To: [log in to unmask]
Subject: [TN] Backward Compatibility of Tin Electroplating


Does anyone have any reason to suspect that tin electroplated SM
components being soldered with a 63/37 solder paste require a profile
that must exceed the reflow temperature of tin?

Being told by a component vendor this is the case.  I would totally
discount this but seem to recall reading this more than once on some
other component Tech data sheets. I can't explain why this would be
necessary, but.....

Any thoughts would be appreciated. 

Rich K / Kimball
  

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

Disclaimer :
The contents of this e-mail including any attachments are intended only
for the person or entity to which this e-mail is addressed.  If you are not,
or believe you may not be, the intended recipient, please advise the sender
immediately by return e-mail, delete this e-mail and destroy any copies.
Tenix does not warrant nor guarantee that this email communication is free
from errors, virus, interception or interference.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2