TECHNET Archives

August 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Charles Barker <[log in to unmask]>
Date:
Sat, 28 Aug 1999 15:59:39 -0500
Content-type:
text/plain; charset=us-ascii
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (57 lines)
How old are the boards, Steve?   FR-4 or Polyimide?

I've seen old boards do that. Suspected moisture entrapment. Never have seen it
with "new" boards.

Charlie B.




Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond to
      [log in to unmask]








 To:      [log in to unmask]

 cc:      (bcc: Charles Barker/US/I-O INC)



 Subject: [TN] Blisters or Delamination after Wave...





Hi ya'll!

Well, I'm in onna Saturday...(Months end, you know how that goes!). Just
finished waving a small lot of boards (9 assemblies) and 5 of them came off
the wave with these dime to quarter-sized delaminated blisters, maybe 3-4 of
them on each board, and the other 4 boards looked fine! What would cause
that? Entrapped moisture? The boards were supposedly baked before wave (At
least the traveler said they were). Any ideas?

-Steve Gregory-

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2