Wade ,
We are using SERA for solderability test of finished PSB before shipment .
This test requested and recognised by some of our customers .
The manufacturer is ECI , their e-mail : [log in to unmask]
The method is recognised by IPC and ex-MILL .
Regards
At 11:53 19/01/99 -0600, you wrote:
>Dear Technetters,
> Does anyone use the SERA technique/equipment for solderability
>testing or evaluation? Dave H at Rockwell seems to be one of the
>experts on this topic. Can Dave or someone else tell me who sells this
>equipment and a phone number and if this equipment is accepted by
>industry?
>
>Regards,
>
>Wade Oberle
>[log in to unmask]
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
>
Edward Szpruch
Eltek Ltd - Israel Tel : 972 - 3 - 9305050 , Fax : 972 - 3 - 9309581
Sgoola industrial Zone , POB 159 , 49101 Petah Tikva , Israel
e-mail : [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|