Wade , We are using SERA for solderability test of finished PSB before shipment . This test requested and recognised by some of our customers . The manufacturer is ECI , their e-mail : [log in to unmask] The method is recognised by IPC and ex-MILL . Regards At 11:53 19/01/99 -0600, you wrote: >Dear Technetters, > Does anyone use the SERA technique/equipment for solderability >testing or evaluation? Dave H at Rockwell seems to be one of the >experts on this topic. Can Dave or someone else tell me who sells this >equipment and a phone number and if this equipment is accepted by >industry? > >Regards, > >Wade Oberle >[log in to unmask] > >################################################################ >TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c >################################################################ >To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: >To subscribe: SUBSCRIBE TechNet <your full name> >To unsubscribe: SIGNOFF TechNet >################################################################ >Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. >For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 >################################################################ > > > Edward Szpruch Eltek Ltd - Israel Tel : 972 - 3 - 9305050 , Fax : 972 - 3 - 9309581 Sgoola industrial Zone , POB 159 , 49101 Petah Tikva , Israel e-mail : [log in to unmask] ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################