I am looking for any and all information on the use of Conductive Carbon /
Silver Ink Polymer Thick Film on PCB card edge contact tabs as a
replacement for the gold plating, (gold fingers). I have information from
Electra on the Electrodor material and from National Starch - Acheson on
the Minico material. Does anyone have experience with use of these
materials on PCB / PWB edge connector contact tabs? I am looking for
electrical, mechanical, reliability, quality, cost, etc. characteristics
comparing conductive PTF to the typical 30 micro-inch gold plating used.
I appreciate and thank you for any information and leads.
[log in to unmask] (512) 723-8481
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|