From a soldering point of view I have a preference for immersion silver.
More generally I understand some people whose products are to be used in
adverse situations contend that any real metal plate offers better
protection to copper against possible corrosion than any organic material.
This is on the tracks as well as unsoldered pads. [And this includes
conformal coat boards and so on.]
Suggest you hope a coating guy is reading this, they are better qualified to
comment on protection offered by resin systems than me.
Regards
Mike Fenner
Indium Corporation
T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Pb-free: www.Pb-Free.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kevin Glidden
Sent: Friday, October 20, 2006 1:59 PM
To: [log in to unmask]
Subject: Re: [TN] Gold immersion vs. silver immersion
Not necessarily...only if the solder wets to the entire pad, which may not
be so if using lead free...
Kevin
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ian Hanna
Sent: Friday, October 20, 2006 8:46 AM
To: [log in to unmask]
Subject: Re: [TN] Gold immersion vs. silver immersion
Assuming you're not assembling at sea -- the finish will have disappeared
into your solder joint long before your ship sails.
Question is do you prefer a copper/solder or a nickel/solder bond. Ian
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Charlie McMahon
Sent: Friday, October 20, 2006 7:28 AM
To: [log in to unmask]
Subject: Re: [TN] Gold immersion vs. silver immersion
Good Morning All:
Might I ask for some guidance from you all..
In determining a surface coating a conflict has arisen between choosing Gold
immersion vs. Silver immersion as the
choice. The application is for boards that are used in shipboard electronics
(non military) but they are protected from the external environment.
My question is which is the more appropriate coating?
Technically, the gold has always worked from the PCB fab and assembly end
with success with a controlled cost of ownership.
The silver however is one that causes concern.
Any suggestions would be appreciated.
Best Regards,
Charlie McMahon
McMahon Sales Company
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
***This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.
Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|