TECHNET Archives

October 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 10 Oct 2006 10:53:46 +0100
Reply-To:
Subject:
From:
Mike Fenner <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (78 lines)
So far as flux is concerned modern low solids no-cleans [are available that]
don't have sufficient resin to block pins so this needn't be an issue.
The max temp of a Pb- wave is not necessarily that much higher than Pb+, but
is worth checking: in this respect I would also be looking to make sure that
the resist/soldermask is Pb- capable. If the resist is not Pb-capable, or
under cured,  it can make a deposit on pads which is very difficult to get
through, This can happen with just heat or combination of some flux solvents
with extra heat on mask can lead to this problem. Have you tried probing an
unfluxed board?


Regards

Mike Fenner
Indium Corporation

T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Pb-free: www.Pb-Free.com



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Thursday, October 05, 2006 7:51 PM
To: [log in to unmask]
Subject: Re: [TN] Lead free ICT testing problems

Are you talking only the ICT bottomside bed of nails fixtures? Then look
at the wave solder flux.
Are you talking about flying probe? Then look at the paste flux.
Are you talking false fails from physically smaller solder joints?
The lead-free solder joints should not be causing any difference in the
probe-ability, unless you are really seeing open solder joints that are
being closed by the probing action.
However, the no-clean flux residues from your Pb-free wave solder
process and reflow process are now probably being "baked on" a little
harder than they were with the no-clean fluxes from your 63/37 process,
as the process temperatures are higher. Thus you get more false fails
because the test pins have a tougher time breaking through the flux
coating.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joel Alexander
Sent: Thursday, October 05, 2006 1:15 PM
To: [log in to unmask]
Subject: [TN] Lead free ICT testing problems

We are seeing intermittent false failures on lead free assemblies. We
would have these occasionally with leaded solder but it has
significantly increased with lead free. We are using SN100C in our wave
solder and Superior 420-S no clean flux.  Are there any types of probe
pins that can produce better yields with lead free solder.



Joel Alexander

APSCO Quality Assurance Manager


***This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.

Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2