TECHNET Archives

November 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 22 Nov 2006 09:07:32 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Dehoyos, Ramon" <[log in to unmask]>
Subject:
From:
"Dehoyos, Ramon" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (48 lines)
        FYI


        Alpha STAR(r)
High Performance Immersion Silver for
Lead-Free Soldering
Consistent reliability in a lead-free circuit board finish just reached
a new level
Includes Alpha STAR Results on Planar Micro void
Issued / Revised: Aug 25, 2006



Surface Finishes Market Trends:

Projected Global Growth and Changes in the Market:  HASL 57%, OSP 20%,
ENIG 14%, ImSn 3% and ImAg 6%  
Projected to be:                                    HASL 37%, OSP 28%,
ENIG 14%, ImSn 4% and ImAg 17% 

CAGR 2004 Global Finish Volume 2008 Global Finish Volume Board Sqft CAGR
HASL -4.4% OSP 14.5% ImAg 42% ImSn 22% ENIG 5.7%

Source: Internal, Prismark, IPC/TMRC*Immersion Silver and OSP will grow
at the expense of HASL and ENIG

*HASL will decline due to the non-uniform planarity, poor cleanliness,
high layer count yield loss, Pb-free cost increase, lack of Pb-free
process development, and industry support

*ENIG high priced contact finish niche will continue, but "Black
Pad"fear, assembler liability issues, and costs pressures will lead to
decline*Immersion 

Tin growth is less clear, press fit preferred, but limited by
inconsistent shelf life, long process time, tin whisker fear and solder
mask compatibility

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2