     Dow Corning makes other RTV's besides the listed ones (which include 
     some conformal coats).
     
     Be prepared to check all RTV's, some are not compatible with copper or 
     tin.


______________________________ Reply Separator _________________________________
Subject: ASM: RTV
Author:  [log in to unmask] at internet
Date:    10/15/96 6:46 PM


Technetters:
  I'm interested in various RTVs that are approved by UL 94-V-0 for flammabil-
ity.  So far I've come up with Dow Corning: 3140, 1-2577/1-2620, 838, 3145 
as well as Sylgard 170 and 567.  In addition, GE Silicones has its RTV133.
     
  Is there anything else out there that can withstand operating temperatures
of at least 125 C and yet remain somewhat rubbery and pliable?
     
Lucy Rojao
[log in to unmask]
     
(416) 448-5866
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To unsubscribe from this list at any time, send a message to:           * 
* [log in to unmask] with <subject: unsubscribe> and no text.        * 
***************************************************************************

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2