The solder temperature range is 235 deg C to 260 deg C. We keep the bath
temperature at 245 deg C.

regards

Sunil Gupta




"Michael.Dorney" <[log in to unmask]> on 22-06-99 19:25:16

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
      to "Michael.Dorney" <[log in to unmask]>

To:   [log in to unmask]
cc:    (bcc: Sunil Gupta/TTL)
Subject:  [TN] Bridging




Hello

I'm working on optimization of a wave solder machine.  There seems to be a
lot of bridging on connectors and I was wondering if the solder temperature
is to low.  Right now it is set at 490oF.  What is the normal temperature
range for wave soldering?

I was also wondering, other than lead length and flux what other factors
might be causing the bridging.

Please send any comments that you have.

Thanks
Mike Dorney