Sunil:
Throwing unwanted solder paste directly into a molten solder bath is a bad
idea. The instantaneous vaporization of fluxes and other ingredients in the
paste results a nasty and volatile reaction.
Ask the paste manufacturer for recommendations.
Bill Kasprzak
Moog Inc.