Hi Dave,
This sounds like a VIPPO (Via In Pad Plated Over)Technology & we do this
a lot for various customers. Yon need to plate the hole, fill it with
epoxy & plate once again to cap the vias to form a pad, so the surface
will be practically flat within +/-2.0mils....
Thanks & Best Regards,
Krishnan C
Director Of Quality
Sanmina-SCI Corporation (M) Sdn. Bhd.
Sama Jaya Free Industrial Zone
93450 Kuching, Sarawak, Malaysia.
Tel: 60 82 363 000 Ext 1602
Mobile: (6) - 012-8888-379
Fax: 60 82 363 527
E-mail: [log in to unmask]
"It is easier to do a job right than to explain why you didn't."
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dave Connitt
Sent: Thursday, October 16, 2008 10:35 PM
To: [log in to unmask]
Subject: Re: [TN] Problems with plating vias closed
Hi Pete,
This is a research/development project. The vias are currently tented,
plus some are under a couple of 100 pin QFP's. I would have to move the
vias out from under the FPGA's or risk solder balls once I untented
them. Since this is a development project, I doubt they will spin the
board again unless there is some other issue. We rarely wave solder
boards anymore as there are very few thru hole parts on them anymore.
The wave was a great way to fill vias with solder. Ah, the good old
days..
Dave Connitt CID+
Printed Circuit Designer
KDI Precision Products, Inc.
A Wholly Owned Subsidiary of:
L3 Communications
3975 McMann Road
Cincinnati, Ohio 45245
Ph. 513- 943-2010 Fax 513-943-2288
-----Original Message-----
From: Pete Houwen [mailto:[log in to unmask]]
Sent: Thursday, October 16, 2008 9:36 AM
To: [log in to unmask]; Connitt, Dave @ KDI
Subject: Re: Problems with plating vias closed
Is this just a matter of closing the holes? Rather than having your PCB
supplier try to plate the holes full, can you let them (partially) fill
during soldering?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
CONFIDENTIALITY
This e-mail message and any attachments thereto, is intended only for use by the addressee(s) named herein and may contain legally privileged and/or confidential information. If you are not the intended recipient of this e-mail message, you are hereby notified that any dissemination, distribution or copying of this e-mail message, and any attachments thereto, is strictly prohibited. If you have received this e-mail message in error, please immediately notify the sender and permanently delete the original and any copies of this email and any prints thereof.
ABSENT AN EXPRESS STATEMENT TO THE CONTRARY HEREINABOVE, THIS E-MAIL IS NOT INTENDED AS A SUBSTITUTE FOR A WRITING. Notwithstanding the Uniform Electronic Transactions Act or the applicability of any other law of similar substance and effect, absent an express statement to the contrary hereinabove, this e-mail message its contents, and any attachments hereto are not intended to represent an offer or acceptance to enter into a contract and are not otherwise intended to bind the sender, Sanmina-SCI Corporation (or any of its subsidiaries), or any other person or entity.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|