Can u illustrate the second point..... I cannot catch the meanings.
Thanks for ur help.
Best Regard,
8/31/99
Mark Mazzoli <[log in to unmask]> on 99/08/30 07:06:09 PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond to
Mark Mazzoli <[log in to unmask]>
To: [log in to unmask]
cc: (bcc: Nicholas LAI/CS/Topsearch)
Subject: Re: [TN] Nick circuit can't detect.. Problem
Hi Nicholas,
Two ideas as to the "dish down" problem. One, they could be resin spots
left on after lamination. They will resist subsequent plating and etching
yet leave the base copper intact after etching. Or, two, plating pits.
They can (and usually do) span the width of the trace (especially if they're
due to air supersaturation in the copper baths). I was unable to open your
attached file so these suggestions are based on your description only.
Good luck
Mark Mazzoli
Eng. Mgr.
Circuit Technologies, Inc.
3622 Clearview Pkwy.
Atlanta, GA 30340
770-458-1700
[log in to unmask]
----- Original Message -----
From: Nicholas LAI <[log in to unmask]>
To: <[log in to unmask]>
Sent: Saturday, August 28, 1999 12:32 AM
Subject: [TN] Nick circuit can't detect.. Problem
>
>
> There is some problems I cannot be solve... Hope all of your can help
me...
>
> (1)We found that there is many board can be escape from E-test...
> After micro-section analysis, we found that there is still base copper on
trace
> open location.
> We can said that the problem is dish down ... There is still connected but
the
> resistance is greater than normal one...
>
> What is the cause of this defect?
> Is there any reliable method to detech it?
> Is there any apparatus can detech the nick circuit problem expect AOI.?
>
> (Embedded image moved to file: pic22705.pcx)
>
> Best Regard,
> nicholas lai
>
>
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|