You can try silver nitrate, I have used it to determine if there is resist left at the foot of
a developed trace. Keep it off your hands, it will stain them and it is used to cauterize
wounds.
Brown, Matthew wrote:
> Does anybody know of a chemical that can be used to detect mono-layers
> of organic resist on top of copper?
> We've had issues in the past with resist residues left after develop
> causing plating problems. A fellow engineer
> mentioned that he had heard of a stain that would leave any contaminated
> areas on the Cu a different color. He
> did not know what it was however...
>
> Matthew Brown
> Metal Plating Engineer
> International Flex Technologies
> Phone: (607) 658-5032
> Pager: (607) 778-4554
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|