TECHNET Archives

March 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Brown, Matthew" <[log in to unmask]>
Date:
Wed, 14 Mar 2001 14:43:04 -0800
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Chuck Brummer <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
From:
Chuck Brummer <[log in to unmask]>
Parts/Attachments:
text/plain (40 lines)
You can try silver nitrate, I have used it to determine if there is resist left at the foot of
a developed trace.  Keep it off your hands, it will stain them and it is used to cauterize
wounds.

Brown, Matthew wrote:

> Does anybody know of a chemical that can be used to detect mono-layers
> of organic resist on top of copper?
> We've had issues in the past with resist residues left after develop
> causing plating problems. A fellow engineer
> mentioned that he had heard of a stain that would leave any contaminated
> areas on the Cu a different color. He
> did not know what it was however...
>
> Matthew Brown
> Metal Plating Engineer
> International Flex Technologies
> Phone: (607) 658-5032
> Pager: (607) 778-4554
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2