TECHNET Archives

December 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Lee parker <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Lee parker <[log in to unmask]>
Date:
Sun, 31 Dec 2006 19:07:13 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (138 lines)
Anil

I was referring to the appearance not the structure, there is of course a 
nickel layer between the copper and gold that is plated on all copper 
features. In most electrolytic gold process the gold/nickel is selectively 
plated of course.

Best regards

Lee

J. Lee Parker, Ph.D.
JLP Consultants LLC
804 779 3389


----- Original Message ----- 
From: "Anil Kher" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Saturday, December 30, 2006 2:29 AM
Subject: Re: [TN] Questions on ENIG VS gold plating


Lee

You are right about flash gold - but 15 mins is Ok to produce 2 um gold and
with variation certain areas can be twice as higher. I have a doubt however
when u say over copper. If it is immersion gold over copper it could be
Uyemura direct immersion gold which can replace enig - and quite non porous
and only on pads and holes. Otherwise it has to be flash electrolytic over 5
um nickel all over the track..

Best wishes and a happy new year to you all.

Anil Kher


-----Original Message-----
From: Lee parker [mailto:[log in to unmask]]
Sent: Saturday, December 30, 2006 3:36 AM
Subject: Re: Questions on ENIG VS gold plating

Werner

If they were using the flash gold chemistry it would require over 12 hours
to plate enough gold to cause an embrittlement problem. I am sure there are
suppliers that use one process and sell it as another. By the way, a
necessary but not sufficient requirement for flash gold is that all copper
features including those under the soldermask be gold plated. Do you recall
if this was the case?

Happy New Year

Lee

J. Lee Parker, Ph.D.
JLP Consultants LLC
804 779 3389


----- Original Message -----
From: "Werner Engelmaier" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, December 29, 2006 3:34 PM
Subject: Re: [TN] Questions on ENIG VS gold plating


Hi Lee,
What I found was significantly more than 2 micro-inches of Au over Ni. It
was
supposed to be electro-plated "flash Au" but sure was certainly much more
than a flash. However, I have no idea what plating chemistry was actually
used—
you know what communicating with a Chinese client regarding another Chinese
vendor is like.


Happy New Year,
Werner

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
----------------------------------------------------- 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

-- 
No virus found in this outgoing message.
Checked by AVG Free Edition.
Version: 7.1.409 / Virus Database: 268.16.0/609 - Release Date: 12/29/2006


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
----------------------------------------------------- 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2