Another interesting article regarding copper-filling microvias.
http://www.enthone-omi.com/electronics/pdf/CAApril03CooksonCopperFill.pdf
Jason Gregory
SMT Production Supervisor/
Integrated Product Team Leader
LaBarge Inc.
(918)459-2367
(918)459-2221 fax
[log in to unmask]
http://www.labarge.com
Carlr Ray
<Carlr.Ray@SANMIN To: [log in to unmask]
A-SCI.COM> cc:
Sent by: TechNet Subject: [TN] BGA Viods
<TechNet@listserv
.ipc.org>
07/02/2003 10:18
AM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to Carlr
Ray
Hello All,
I have a question (more like a poll I guess), concerning voiding of
BGA devices.
I have PBGA 480 IO paremeter grid device and I am seeing lots of
voiding. Per the x-ray I am well within the IPC spec of 35% but I am
still having failures at ICT (OPENS). Once I reviewed the profile I
noticed we were not hitting the dewell time for flux activiation
recommended by the solder paste vender (min 60 seconds) and we were
seeing an extended time above 183c. We have changed the profile but some
of my companions feel that the size of the pad and amount of solder
paste is effecting the voiding. I disagree with them and feel that not
activiating the fluxes and extended time above liquidous is a major
contibutor to the voids.
So now my question, what impact does the pads have with the voiding
of the spheres on the BGA?
Carl Ray
Sr. Manufacturing Engineer
Huntsville, AL 35807
Phone: 256-882-4800 ext. 8845
Cell: 256-990-1990
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|