There are some guidelines in the fine Technet archives.
Dave Fish
----- Original Message -----
From: "Dave Snyder" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, June 07, 2002 2:48 PM
Subject: [TN] Glue or Not to Glue?
> When running SMT boards thru an IR reflow oven are there any guidelines,
IPC
> documents, gut feelings that tell whether gluing is necessary for parts
that
> would be on the bottom side during the top side reflow? I have at least
one
> 160 pin TQFP that would be on the bottom. Is there a formula like mass
> versus total pin area?
>
> Thanks in advance for the advice.
>
> Dave Snyder
> HM Electronics, Inc.
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|