TECHNET Archives

March 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Joel Mearig <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Joel Mearig <[log in to unmask]>
Date:
Mon, 13 Mar 2006 14:57:45 -0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (227 lines)
Just to close the loop on an old thread.

I have decided to use the Teka connectors as they are now supplied lead
free. The connectors are only supplied in a no-clean flux configuration but
I have been running them through a water wash system with no adverse
affects.

The biggest challenge is to get a profile that will reflow the connector
solder and not be too hot for the balance of the SMT components. It has been
working OK to date. I expect better results as I increase the volume of
parts to get a good sample size to do additional process development.

Joel Mearig
Delta Tau Data Systems, Inc.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, October 04, 2005 10:30 AM
To: [log in to unmask]
Subject: Re: [TN] Hand Soldering Long Gold Pins

WHOOPS! I meant PC104.....

I read a couple of later posts, and you said that you are
lead free...that pretty much eliminates my suggestion.

I use connectors from Teka (http://www.takais.com) they
have something they call "Solder-bearing Lead Technology"
with solder pre-forms and flux incorporated into each lead that
you can reflow. But they only have tin/lead preforms.

But you might check with them to see if they are thinking about
doing lead-free connectors.

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX



|---------+---------------------------->
|         |           Joel Mearig      |
|         |           <jmearig@deltatau|
|         |           .com>            |
|         |                            |
|         |           10/04/2005 11:40 |
|         |           AM               |
|         |                            |
|---------+---------------------------->

>---------------------------------------------------------------------------
-----------------------------------|
  |
|
  |       To:       TechNet E-Mail Forum <[log in to unmask]>@SMTP@Exchange,
Stephen R Gregory/LABARGE@LABARGE      |
  |       cc:
|
  |       Subject:  RE: [TN] Hand Soldering Long Gold Pins
|

>---------------------------------------------------------------------------
-----------------------------------|



Steve,
We call it a PC104 design. Is that the same as PC105?       Joel

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, October 04, 2005 9:26 AM
To: [log in to unmask]
Subject: Re: [TN] Hand Soldering Long Gold Pins

Hi Joel!

These pins wouldn't be on a PC105 standard
assembly would they?

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX


|---------+---------------------------->
|         |           Joel Mearig      |
|         |           <jmearig@DELTATAU|
|         |           .COM>            |
|         |           Sent by: TechNet |
|         |           <[log in to unmask]>|
|         |                            |
|         |                            |
|         |           10/04/2005 10:58 |
|         |           AM               |
|         |           Please respond to|
|         |           TechNet E-Mail   |
|         |           Forum            |
|         |           <[log in to unmask]>|
|         |           ; Please respond |
|         |           to Joel Mearig   |
|         |           <jmearig@DELTATAU|
|         |           .COM>            |
|         |                            |
|---------+---------------------------->

>
---------------------------------------------------------------------------
-----------------------------------|
  |
|
  |       To:       [log in to unmask]@SMTP@Exchange
|
  |       cc:       (bcc: Stephen R Gregory/LABARGE)
|
  |       Subject:  [TN] Hand Soldering Long Gold Pins
|

>
---------------------------------------------------------------------------
-----------------------------------|



I have a number of assemblies that have long (0.5") connector pins that
must
be soldered in the board. The pins must remain gold so at the moment I am
trying to hand solder. This is a difficult process. The 0.100" spacing
makes
it difficult for my production personnel to solder without getting solder
on
the gold pins.



The connectors are double row and there are two beside one another creating
a four pin bank of 0.100" spaced pins. Any thoughts on how I can improve
this process for the soldering personnel would be greatly appreciated.



Joel Mearig




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------



__________________________________________________________________
This message may contain information that is privileged and confidential to
LaBarge, Inc.  It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone.  In such event, you should destroy the message and
kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------




__________________________________________________________________
This message may contain information that is privileged and confidential to
LaBarge, Inc.  It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone.  In such event, you should destroy the message and
kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2