Just to close the loop on an old thread. I have decided to use the Teka connectors as they are now supplied lead free. The connectors are only supplied in a no-clean flux configuration but I have been running them through a water wash system with no adverse affects. The biggest challenge is to get a profile that will reflow the connector solder and not be too hot for the balance of the SMT components. It has been working OK to date. I expect better results as I increase the volume of parts to get a good sample size to do additional process development. Joel Mearig Delta Tau Data Systems, Inc. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory Sent: Tuesday, October 04, 2005 10:30 AM To: [log in to unmask] Subject: Re: [TN] Hand Soldering Long Gold Pins WHOOPS! I meant PC104..... I read a couple of later posts, and you said that you are lead free...that pretty much eliminates my suggestion. I use connectors from Teka (http://www.takais.com) they have something they call "Solder-bearing Lead Technology" with solder pre-forms and flux incorporated into each lead that you can reflow. But they only have tin/lead preforms. But you might check with them to see if they are thinking about doing lead-free connectors. Kind regards, -Steve Gregory- Senior Process Engineer LaBarge Incorporated Tulsa, Oklahoma (918) 459-2285 (918) 459-2350 FAX |---------+----------------------------> | | Joel Mearig | | | <jmearig@deltatau| | | .com> | | | | | | 10/04/2005 11:40 | | | AM | | | | |---------+----------------------------> >--------------------------------------------------------------------------- -----------------------------------| | | | To: TechNet E-Mail Forum <[log in to unmask]>@SMTP@Exchange, Stephen R Gregory/LABARGE@LABARGE | | cc: | | Subject: RE: [TN] Hand Soldering Long Gold Pins | >--------------------------------------------------------------------------- -----------------------------------| Steve, We call it a PC104 design. Is that the same as PC105? Joel -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory Sent: Tuesday, October 04, 2005 9:26 AM To: [log in to unmask] Subject: Re: [TN] Hand Soldering Long Gold Pins Hi Joel! These pins wouldn't be on a PC105 standard assembly would they? Kind regards, -Steve Gregory- Senior Process Engineer LaBarge Incorporated Tulsa, Oklahoma (918) 459-2285 (918) 459-2350 FAX |---------+----------------------------> | | Joel Mearig | | | <jmearig@DELTATAU| | | .COM> | | | Sent by: TechNet | | | <[log in to unmask]>| | | | | | | | | 10/04/2005 10:58 | | | AM | | | Please respond to| | | TechNet E-Mail | | | Forum | | | <[log in to unmask]>| | | ; Please respond | | | to Joel Mearig | | | <jmearig@DELTATAU| | | .COM> | | | | |---------+----------------------------> > --------------------------------------------------------------------------- -----------------------------------| | | | To: [log in to unmask]@SMTP@Exchange | | cc: (bcc: Stephen R Gregory/LABARGE) | | Subject: [TN] Hand Soldering Long Gold Pins | > --------------------------------------------------------------------------- -----------------------------------| I have a number of assemblies that have long (0.5") connector pins that must be soldered in the board. The pins must remain gold so at the moment I am trying to hand solder. This is a difficult process. The 0.100" spacing makes it difficult for my production personnel to solder without getting solder on the gold pins. The connectors are double row and there are two beside one another creating a four pin bank of 0.100" spaced pins. Any thoughts on how I can improve this process for the soldering personnel would be greatly appreciated. Joel Mearig --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- __________________________________________________________________ This message may contain information that is privileged and confidential to LaBarge, Inc. It is for use only by the individual or entity named above. If you are not the intended recipient, you may not copy, use or deliver this message to anyone. In such event, you should destroy the message and kindly notify the sender by reply e-mail. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- __________________________________________________________________ This message may contain information that is privileged and confidential to LaBarge, Inc. It is for use only by the individual or entity named above. If you are not the intended recipient, you may not copy, use or deliver this message to anyone. In such event, you should destroy the message and kindly notify the sender by reply e-mail. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------