TECHNET Archives

February 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vvYKT-0000aMC; Fri, 14 Feb 97 18:50 CST
Disclose-recipients:
prohibited
Old-Return-Path:
Date:
Fri, 14 Feb 1997 07:19:00 -0500 (EST)
MIME-version:
1.0
Precedence:
list
X400-MTS-identifier:
[;23527041207991/307616@ALLIN1]
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
Priority:
normal
X-Loop:
X-Mailing-List:
<[log in to unmask]> archive/latest/10265
Resent-From:
Alternate-recipient:
prohibited
Resent-Message-ID:
<"p5_nC1.0.Z1L.0XG1p"@ipc>
Return-Path:
<TechNet-request>
Subject:
A1-type:
MAIL
Message-id:
MR-Received:
by mta ALLIN1; Relayed; Fri, 14 Feb 1997 07:25:32 -0500
Content-type:
TEXT/PLAIN; CHARSET=US-ASCII
From [log in to unmask] Tue Feb 18 09:
32:29 1997
From:
Jim Marsico 516-595-5879 <[log in to unmask]>
Posting-date:
Fri, 14 Feb 1997 07:25:00 -0500 (EST)
Hop-count:
1
Importance:
normal
TO:
Parts/Attachments:
TEXT/PLAIN (34 lines)
Dear Technet:

A prominent component manufacturer uses a Pb46 Sn46 Bi8 alloy for the balls on 
BGAs.  Can anyone think of any problems soldering these with Sn63 solder paste? 
Any metallurgical or reliability issues?

Thanks

Jim Marsico
(516) 595-5879
[log in to unmask]
		
                        ********************************
                        *       ______   _   _  _____  *
                        *      / ___  | | | | | _____  *
                        *     / /___| | | | | | _____  *
                        *  __/  ____  | | | | |______  * 
                        * |____/    |_| |_| |________| *
                        *                              *
                        *         SYSTEMS, INC.        *
                        ********************************

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2