TECHNET Archives

February 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vxAC1-0000gQC; Wed, 19 Feb 97 05:28 CST
Encoding:
55 Text
Old-Return-Path:
Date:
Wed, 19 Feb 97 05:35:58 cst
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/10360
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"LjSDC.0.uF9.8Fk2p"@ipc>
Subject:
From:
"ddhillma" <[log in to unmask]>
X-Loop:
From [log in to unmask] Wed Feb 19 12:
14:21 1997
Message-Id:
Parts/Attachments:
text/plain (68 lines)
     Hi Jim-
     
     Several of the Sn/Pb/Bi solder alloys have "hot shortness" problems at 
     98C (a eutectic melting point). I believe that some information 
     covering Sn/Pb/Bi alloys will be covered at IPC Expo on Tuesday 
     morning as part of the NCMS Lead Free technical session. I know of 
     several Sn/Pb/Bi alloys in industry use (43Sn/43Pb/14Bi the most 
     prevalent) but they all have use environments below 98 C. I would do 
     some testing in your use environment to see if reliability problems 
     arise.
     
     
     Dave Hillman
     Rockwell Collins
     [log in to unmask]


______________________________ Reply Separator _________________________________
Subject: ASSY: SOLDER ALLOYS AND BGAs
Author:  [log in to unmask] at ccmgw1
Date:    2/15/97 9:50 AM


Dear Technet:
     
A prominent component manufacturer uses a Pb46 Sn46 Bi8 alloy for the balls on 
BGAs.  Can anyone think of any problems soldering these with Sn63 solder paste? 
Any metallurgical or reliability issues?
     
Thanks
     
Jim Marsico
(516) 595-5879
[log in to unmask]
     
                        ********************************
                        *       ______   _   _  _____  *
                        *      / ___  | | | | | _____  *
                        *     / /___| | | | | | _____  *
                        *  __/  ____  | | | | |______  * 
                        * |____/    |_| |_| |________| *
                        *                              *
                        *         SYSTEMS, INC.        *
                        ********************************
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   * 
* with <subject: subscribe/unsubscribe> and no text in the body.          * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************