TECHNET Archives

June 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Ken Patel <[log in to unmask]>
Date:
Wed, 16 Jun 2004 22:18:21 -0700
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, David Douthit <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii; format=flowed
From:
David Douthit <[log in to unmask]>
Parts/Attachments:
text/plain (108 lines)
Ken,

Exposure to 288 degrees C for a period of time (T260 = 260 degrees C
exposure).

David A. Douthit
Manager
LoCan LLC

Ken Patel wrote:

>Gerard,
>HASL - I meant eutectic solder (63/37).
>
>What does it mean T288 performance?
>
>Re,
>Ken Patel
>
>-----Original Message-----
>From: Gerard O'Brien [mailto:[log in to unmask]]
>Sent: Wednesday, June 16, 2004 5:05 AM
>To: TechNet E-Mail Forum.; Ken Patel
>Subject: RE: [TN] Lead-free Assy process and fab surface finish
>
>Ken - depending on the OSP coating being used and the flux activation levels
>- you may be forced into N2 atmosphere. For ENIG we have seen no problems.
>For HASL - do you mean a lead free alloy?
>
>
>The Tg of the material is NOT as critical as the T288 performance. A
>laminate with a T288 of 15+ minutes will provide you all the necessary
>performance needed for Pb free assembly. There are many Tg 170 materials out
>there that have excellent T260 results but blow up ever before reaching
>288C.
>
>Regards
>
>
>Gerard O'Brien
>Photocircuits Corporation
>
>-----Original Message-----
>From: Ken Patel [mailto:[log in to unmask]]
>Sent: Tuesday, June 15, 2004 4:07 PM
>To: [log in to unmask]
>Subject: [TN] Lead-free Assy process and fab surface finish
>
>Technetters,
>
>I do have few questions related to fab surface finish in lead-free assembly
>environment.
>
>
>
>(1)Do you see any problem with board surface finishes, particularly OSP,
>HASL, and Nickel-Gold?
>
>
>
>(2) What should be the minimum Tg of Fab material? Is Tg of >170C is good
>enough?
>
>
>
>Re,
>
>Ken Patel
>
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
>-----------------------------------------------------
>
>
>
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2