TECHNET Archives

May 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Adam Seychell <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Adam Seychell <[log in to unmask]>
Date:
Wed, 2 May 2007 17:46:49 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (34 lines)
On Mon, 30 Apr 2007 09:14:23 -0400, DDFRITZ <[log in to unmask]> wrote:

....
>Direct metallization will work on the holes and microvias with all these
techniques, but it will not work well with the third alternative above.  The
"knit rate" for copper electroplate over direct metallization is not fast
enough for most horizontal platers, and if you have NO foil on the board,
where do you start the copper electroplate from?  Direct metallization works
fine where you have two starting sheets of copper foil and only have to knit
the holes.  But it is exceedingly difficult where the is no starting foil
anywhere on the surface.
>
>

This is what I expected. I am not sure what the physical rate of the copper
growth front is for direct metalization ("knit rate"), but I suspect even if
one were to make several cathode contact points on the panel perimeter, then
it will just be too slow. And even if it could metallize the work piece,
there will be the adhesion problem as you say. 
Roughly how much time does it take to plate the wall of a 1.6mm length hole
using direct metallization ?  30s, 60s, 5min ? 

Adam

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2