On Mon, 30 Apr 2007 09:14:23 -0400, DDFRITZ <[log in to unmask]> wrote: .... >Direct metallization will work on the holes and microvias with all these techniques, but it will not work well with the third alternative above. The "knit rate" for copper electroplate over direct metallization is not fast enough for most horizontal platers, and if you have NO foil on the board, where do you start the copper electroplate from? Direct metallization works fine where you have two starting sheets of copper foil and only have to knit the holes. But it is exceedingly difficult where the is no starting foil anywhere on the surface. > > This is what I expected. I am not sure what the physical rate of the copper growth front is for direct metalization ("knit rate"), but I suspect even if one were to make several cathode contact points on the panel perimeter, then it will just be too slow. And even if it could metallize the work piece, there will be the adhesion problem as you say. Roughly how much time does it take to plate the wall of a 1.6mm length hole using direct metallization ? 30s, 60s, 5min ? Adam --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------