TECHNET Archives

March 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Barmuta, Michael" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Barmuta, Michael
Date:
Wed, 21 Mar 2007 08:58:44 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (95 lines)
Hi Jack: A couple of questions.
1. What is the capacity of the solderpot?
2. What is the flux being used?
3. What is the material the pot is made of? 
4. Does the problem show up on a new pot charge or does it require time
to develop if so how long?
5. What is your definition of "polarized metal stuff"? Are you saying
magnetic or are we getting into dipole moments and ligand field theory?

	
Regards
	
Michael Barmuta
	
Staff Engineer
	
Fluke Corp.
	
Everett WA
	
425-446-6076

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Evans
Sent: Wednesday, March 21, 2007 8:57 AM
To: [log in to unmask]
Subject: [TN] Whisker contamination is solder pot

Hi Folks,
We use a small solder pot with a nitrogen atmosphere to pre tin
components. 
We are using Kester ultra pure 63/37 bar solder at 260C (500F) and
tinning in 
the neighborhood of 500 components per month, then the solder is
changed. 
The problem that we are seeing is some kind of contamination in the way
of 
very small, fine, hairlike, polarized metal stuff.  Analysis of this
stuff claims 
that it is copper or iron, but we can't get a real good sample to know
exactly 
what it is. Kester has been sent samples and they have come back with 
nothing and I have had an outside lab, as well as our own look at this
solder 
with nothing definitive as to what it is or where it comes from.  I have
tried 
three different lots of solder and the problem continues to show up on
a 
random basis. Our tinning pot is obsolete and I can't go our and buy a
new 
pot, so that option is not available.  Just wondering if anyone else has
ran into 
this problem and possibly found a solution?

Thanks,
Jack Evans,
Aeroflex Colorado Springs

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

This message (including any attachments) contains confidential 
and/or proprietary information intended only for the addressee.  
Any unauthorized disclosure, copying, distribution or reliance on 
the contents of this information is strictly prohibited and may 
constitute a violation of law.  If you are not the intended 
recipient, please notify the sender immediately by responding to 
this e-mail, and delete the message from your system.  If you 
have any questions about this e-mail please notify the sender 
immediately. 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2