HI Gaby
I really need a metallurgist to tell me what I think when looking at X
sections, but I think I see two conditions:
Small1, small2 are pretty homogenous, just look like a little too low too
shot TAL ,
Small Small3 small4 are not homogenous and show evidence of cracking/HIP
Probably are mixed alloy.
All pictures have stuff in them, whether this is a construct from section or
inclusions of flux etc I can't tell, but the big dark features which look
like cracks at first sight are probably not cracks, they are not "cracky
enough". Shrinks or blow holes I would guess.


Regards
 
 
Mike
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gabriela
Sent: 04 July 2009 08:54
To: [log in to unmask]
Subject: [TN] Weird solder joints

Dear all,
By cross sectioning BGA solder joints on a failed assembly, I found that the
suspected joints are not uniform and that they contain unusual separation
areas.

I suspect mixed assembly and/or bad reflow profile.

Steve was so kind and enabled me to send the links.
Please may I have your opinion?
http://stevezeva.homestead.com/files/small.jpg

 

 <http://stevezeva.homestead.com/files/small1.jpg>
http://stevezeva.homestead.com/files/small1.jpg

 

 <http://stevezeva.homestead.com/files/small2.jpg>
http://stevezeva.homestead.com/files/small2.jpg

http://stevezeva.homestead.com/files/small3.jpg

 <http://stevezeva.homestead.com/files/small4.jpg>
http://stevezeva.homestead.com/files/small4.jpg

 


Gaby


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


***This email, its content, and any files transmitted with it, are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient, please contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination, or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited.

Messages sent via this medium may be subjected to delays, non-delivery, and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. Indium Corporation does not accept responsibility for changes made to this email after is was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2