TECHNET Archives

November 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Ingemar Hernefjord <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Ingemar Hernefjord <[log in to unmask]>
Date:
Wed, 23 Nov 2005 14:43:28 +0100
Content-Type:
text/plain
Parts/Attachments:
text/plain (137 lines)
Gil,

We have been soldering even larger parts for microwave use. There are
two alternative ways, if you are lucky to have those possibilites:
a) fluxless soldering preform and soldering in a vacuum oven.
b) ditto in a nitrogen oven
In both cases we cleaned the lands (pads)and the preform in a weak
acidous (formic acid) solution immediately before soldering, and cleaned
the part in deionised water afterwards.

Ingemar Hernefjord
Ericsson Microwave Systems

-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Zilber Gil
Skickat: den 23 november 2005 13:01
Till: [log in to unmask]
Ämne: Re: [TN] Unusual soldering challenge

Hello Jeff,

We had similar components short time ago, and we create a grid in the
aperture of the stencil, similar to what Ivan suggested. The reflow pass
well, but after examine the component with X-ray we saw air trapped in
the solder (about 20% of the area). Thus, I suggest designing the pad on
the PCB the same way as the grid in the stencil.

Regards,

Gil Zilber
Technologist, Elta system Ltd.
Tel. +972-8-8577240
Mobile +972-54-4983222
http://www.iai.co.il/site/en/iai.asp?pi=17887


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jeff Brown
Sent: Tuesday, November 22, 2005 7:46 AM
To: [log in to unmask]
Subject: [TN] Unusual soldering challenge

Hi Everyone,

We have a problem with a fairly unique component that requires soldering
to a PCB. I'm really hoping that someone has seen this before as it
looking really awkward.

The component is mounted on a piece of fiberglass about 25mm x 16mm. The
footprint consists of a ground pad which takes up 95% of the area, and
four signal pads with 0.5mm clearance from the ground pad.

The manufacturer recommends a grid of stenciled paste for the ground pad
due to the large area, but we are concerned that if the paste melts from
the outside edges in, then it will at a minimum result in flux
entrapment, and at worst, the trapped flux will boil and lift the
component, or move the molten solder causing shorts to the signal pads.

I imagine that even if we used solid paste pattern that this would
probably only make the problem worse.

Or are we just being overly pessimistic?

Any thoughts on options would be gratefully received...  Currently
wondering about the possibility of applying BGA balls to the package so
that there is some clearance between the board and the component.

If anyone is interested, I can send the component datasheet to them
directly.

Thank you all in advance

Jeff Brown and Josh Vear
EOS Space Systems

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


This message is processed by the PrivaWall Email Security Server.





 The information contained in this communication is proprietary to
Israel Aircraft Industries Ltd.
and/or third parties, may contain confidential or privileged
information, and is intended only for
the use of the intended addressee thereof. If you are not the intended
addressee, please be aware
that any use, disclosure, distribution and/or copying of this
communication is strictly prohibited.
If you receive this communication in error, please notify the sender
immediately and delete it from
your computer. Thank you.


This message is processed by the PrivaWall Email Security Server.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2