I believe some washing difficulties relate to how dry the masks get.
They have to be rehydrated before washing off, so if too dry, this can
take a longer time. Most of them have constituents which help keep some
moisture in them, but time and temperature will increase dryness.
Regards,
Peter
--------------------------------------------------------
Peter Swanson [log in to unmask]
INTERTRONICS http://www.intertronics.co.uk
Tel: +44 1865 842842 Oxfordshire, England
INTERTRONICS is dedicated to providing quality material, consumable
and equipment solutions to the high technology, high performance
assembly industries, incorporating outstanding levels of technical
support and customer service.
Read our news! http://www.intertronics.co.uk/blog/blog.htm
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: 23 May 2008 21:10
To: [log in to unmask]
Subject: Re: [TN] Water soluble masking
Hi Ioan!
We use Techspray (the light blue stuff) here, and don't have any
problems. We even mask boards on Friday, leave them set over the
weekend, then wave them Monday, and they clean fine for us. We have a
Technical Devices In-line cleaner running deionized water at about 150
F., at a belt speed of around 4 fpm, and haven't had any problems.
There's even been a few occasions that boards have been accidently left
in a 180 F. oven (meant to speed the cure of the mask) over the weekend
and they have still cleaned fine after wave.
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: Friday, May 23, 2008 2:53 PM
To: [log in to unmask]
Subject: [TN] Water soluble masking
Dear Technos,
I am testing WS solder masking substances and what I see is that they
wash perfectly if relatively fresh (barely cured or after a couple of
hours on the board) and they wash very poorly if passed in the in-line
machine 24 or 48 hours after the application.
Is this natural? What is your experience?
Chemtronics have a note on the bottle requesting washing within 48
hours, nothing marked on the Techspray bottle, but both are very
difficult to remove after 24 hours.
Thanks,
Ioan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|